Skip to content

💎测得物性

工程陶瓷 · 用于热、磨损与电子的晶态氧化物与碳化物——不是桌上的杯子。

Numbers below are bands used by working engineers, not live quotes. Tensile note: high compressive; tensile limited by flaws (Weibull).

Fire performance in this atlas is editorial. Real projects need the assembly report.

力学

Strength band

high compressive; tensile limited by flaws (Weibull)

Stiffness

Modulus follows chemistry and orientation — not the marketing nickname.

Toughness

Crack growth, not peak stress, retires most real parts.

Fatigue / creep

Cyclic and time-dependent damage dominate certificates issued on static coupons.

Hardness / hand

Indentation, drape or compressive class — whichever the trade actually measures.

热学

Conductivity

Al2O3 ~20–30; AlN higher; ZrO2 low — 工程陶瓷 is not a substitute for a dedicated λ layer.

Service temperature

Melting / softening / decomposition band: often >2000 °C.

Expansion

Joints and clearances must follow the expansion class of 工程陶瓷, not of steel-by-habit.

Thermal mass

Density 3.2–6 g/cm³ class sets how fast a section changes temperature.

Ageing of λ

Foams, VIPs and moist batts drift; quote aged values.

电学

Conductor or dielectric

工程陶瓷 is generally a dielectric or semiconductor film, not building wire.

Static / EMI

Fillers and moisture change resistivity more than brochures admit.

Standards language

IACS, volume resistivity or dielectric strength — pick the quantity the job uses.

火灾

Reaction to fire

Typical declared class: A1. This is not a universal passport.

Resistance vs reaction

Euroclass is reaction. EI/R ratings are assemblies — boards, coats, cavities.

Melt-drip / char

工程陶瓷 tends to char or stay inorganic rather than melt-drip like commodity olefins.

Smoke / toxicity

CO, HCN, HF or fibres — the species depend on chemistry. Name the test (ISO 5659, EN 45545, NFPA 1971).

If a salesperson quotes a single “safety score”, ask which standard, which thickness, which year.

继续浏览

陶瓷与木材中的其他材料