본문으로 건너뛰기

🩺측정 물성

니티놀 · 형상을 기억하고 초탄성하는 거의 등원자 Ni–Ti — 스텐트, 교정, 액추에이터.

Numbers below are bands used by working engineers, not live quotes. Tensile note: superelastic plateau ~400–600 MPa class, cycle dependent.

Fire performance in this atlas is editorial. Real projects need the assembly report.

기계적

Strength band

superelastic plateau ~400–600 MPa class, cycle dependent

Stiffness

Modulus follows chemistry and orientation — not the marketing nickname.

Toughness

Crack growth, not peak stress, retires most real parts.

Fatigue / creep

Cyclic and time-dependent damage dominate certificates issued on static coupons.

Hardness / hand

Indentation, drape or compressive class — whichever the trade actually measures.

Conductivity

~10–18 W/m·K — 니티놀 is not a substitute for a dedicated λ layer.

Service temperature

Melting / softening / decomposition band: ~1310 °C.

Expansion

Joints and clearances must follow the expansion class of 니티놀, not of steel-by-habit.

Thermal mass

Density ~6.45 g/cm³ sets how fast a section changes temperature.

Ageing of λ

Foams, VIPs and moist batts drift; quote aged values.

전기

Conductor or dielectric

니티놀 is generally a dielectric or semiconductor film, not building wire.

Static / EMI

Fillers and moisture change resistivity more than brochures admit.

Standards language

IACS, volume resistivity or dielectric strength — pick the quantity the job uses.

화재

Reaction to fire

Typical declared class: A1 metal. This is not a universal passport.

Resistance vs reaction

Euroclass is reaction. EI/R ratings are assemblies — boards, coats, cavities.

Melt-drip / char

니티놀 tends to char or stay inorganic rather than melt-drip like commodity olefins.

Smoke / toxicity

CO, HCN, HF or fibres — the species depend on chemistry. Name the test (ISO 5659, EN 45545, NFPA 1971).

If a salesperson quotes a single “safety score”, ask which standard, which thickness, which year.

계속 둘러보기