본문으로 건너뛰기

🏠측정 물성

석고보드 · 탈수로 화재 시간을 사는 이수석고 패널 — 실내의 일상 A2/A1 마감.

Numbers below are bands used by working engineers, not live quotes. Tensile note: paper faces take bending; wet boards are scrap.

Fire performance in this atlas is editorial. Real projects need the assembly report.

기계적

Strength band

paper faces take bending; wet boards are scrap

Stiffness

Modulus follows chemistry and orientation — not the marketing nickname.

Toughness

Crack growth, not peak stress, retires most real parts.

Fatigue / creep

Cyclic and time-dependent damage dominate certificates issued on static coupons.

Hardness / hand

Indentation, drape or compressive class — whichever the trade actually measures.

Conductivity

~0.17 W/m·K — 석고보드 is not a substitute for a dedicated λ layer.

Service temperature

Melting / softening / decomposition band: calcines ~80–180 °C (dehydration).

Expansion

Joints and clearances must follow the expansion class of 석고보드, not of steel-by-habit.

Thermal mass

Density ~700–1000 kg/m³ sets how fast a section changes temperature.

Ageing of λ

Foams, VIPs and moist batts drift; quote aged values.

전기

Conductor or dielectric

석고보드 is generally a dielectric or semiconductor film, not building wire.

Static / EMI

Fillers and moisture change resistivity more than brochures admit.

Standards language

IACS, volume resistivity or dielectric strength — pick the quantity the job uses.

화재

Reaction to fire

Typical declared class: A2-s1,d0 typical; core A1. This is not a universal passport.

Resistance vs reaction

Euroclass is reaction. EI/R ratings are assemblies — boards, coats, cavities.

Melt-drip / char

석고보드 tends to char or stay inorganic rather than melt-drip like commodity olefins.

Smoke / toxicity

CO, HCN, HF or fibres — the species depend on chemistry. Name the test (ISO 5659, EN 45545, NFPA 1971).

If a salesperson quotes a single “safety score”, ask which standard, which thickness, which year.