Strength band
modest vs NR; stability is the product
실리콘 · Si–O 골격 엘라스토머·수지 — 베이크웨어, 의료 튜브, 실란트, 탄소 사슬보다 고온에 관대.
Numbers below are bands used by working engineers, not live quotes. Tensile note: modest vs NR; stability is the product.
Fire performance in this atlas is editorial. Real projects need the assembly report.
modest vs NR; stability is the product
Modulus follows chemistry and orientation — not the marketing nickname.
Crack growth, not peak stress, retires most real parts.
Cyclic and time-dependent damage dominate certificates issued on static coupons.
Indentation, drape or compressive class — whichever the trade actually measures.
~0.2 W/m·K; filled greases conduct — 실리콘 is not a substitute for a dedicated λ layer.
Melting / softening / decomposition band: elastomer; resins cure.
Joints and clearances must follow the expansion class of 실리콘, not of steel-by-habit.
Density ~1.1–1.5 g/cm³ sets how fast a section changes temperature.
Foams, VIPs and moist batts drift; quote aged values.
실리콘 is generally a dielectric or semiconductor film, not building wire.
Fillers and moisture change resistivity more than brochures admit.
IACS, volume resistivity or dielectric strength — pick the quantity the job uses.
Typical declared class: often high LOI vs organic rubbers. This is not a universal passport.
Euroclass is reaction. EI/R ratings are assemblies — boards, coats, cavities.
실리콘 can burn or drip; do not treat it as A1 without a system test.
CO, HCN, HF or fibres — the species depend on chemistry. Name the test (ISO 5659, EN 45545, NFPA 1971).
If a salesperson quotes a single “safety score”, ask which standard, which thickness, which year.