Strength band
high compression, low tension; tempering stores surface compression
유리 · 얼어붙은 규산염 액체 — 창, 병, 섬유. A1이지만 깨지고 화재에 연화한다.
Numbers below are bands used by working engineers, not live quotes. Tensile note: high compression, low tension; tempering stores surface compression.
Fire performance in this atlas is editorial. Real projects need the assembly report.
high compression, low tension; tempering stores surface compression
Modulus follows chemistry and orientation — not the marketing nickname.
Crack growth, not peak stress, retires most real parts.
Cyclic and time-dependent damage dominate certificates issued on static coupons.
Indentation, drape or compressive class — whichever the trade actually measures.
~1 W/m·K — 유리 is not a substitute for a dedicated λ layer.
Melting / softening / decomposition band: softens ~500–700 °C.
Joints and clearances must follow the expansion class of 유리, not of steel-by-habit.
Density ~2.5 g/cm³ sets how fast a section changes temperature.
Foams, VIPs and moist batts drift; quote aged values.
유리 is generally a dielectric or semiconductor film, not building wire.
Fillers and moisture change resistivity more than brochures admit.
IACS, volume resistivity or dielectric strength — pick the quantity the job uses.
Typical declared class: A1. This is not a universal passport.
Euroclass is reaction. EI/R ratings are assemblies — boards, coats, cavities.
유리 tends to char or stay inorganic rather than melt-drip like commodity olefins.
CO, HCN, HF or fibres — the species depend on chemistry. Name the test (ISO 5659, EN 45545, NFPA 1971).
If a salesperson quotes a single “safety score”, ask which standard, which thickness, which year.